Main parameters
Before tansformation
After transformation
Coal consumption at kiln head(t/h)
6.1-6.5
5.6-6
Coal consumption at kiln tail(t/h)
8.4-9.2
8-8.4
Kiln feeding(t/h)
190
190
Secondary air temperature(℃)
980-1040
980-1040
Tertiary air temperature(℃)
820-880
840-890
C1 outlet temperature(℃)
320-345
320-340
Kiln tail temperature(℃)
1010-1100
1005-1080
NOx standard(mg/Nm³)
Below 400
Below 400
NOx actural emission(mg/Nm³)
330-390
55-96
Ammonia consumption(m³/h)
646-720
563-636
O2 emission(%)
7.4-8
6.9-7.2
Clinker KH value
0.920
0.920
Clinker 3 days strength(MPa)
34
34
Clinker 28 days strength(MPa)
Updating
Updating
Clinker standard coal(kg/t)
Updating
Updating