Technical parmaters
Before transformation
After transformation
Coal consumption at kiln head(t/h)
17
17
Coal consumption at kiln tail(t/h)
22
22
Kiln feeding(t/h)
500
500
Secondary air temperature(℃)
1150
1180
Tertiary air temperature(℃)
900
930
C1 outlet temperature(℃)
320
310
Kiln tail temperature(℃)
1180
1150
NOx standard(mg/Nm³)
260
100
NOx actural Emission(mg/Nm³)
150
100
Ammonia consumption(m³/h)
1.2
0.8
O2 emission(%)
8
8
Clinker KH value
0.90
0.90
Clinker 3 days strength(MPa)
32
32